Thursday, February 18, 2010

Ashes to Ashes....

Dust to Dust......


OR


The Unfortunate Matt Fiberglass Fiasco......


This is what 2 square yards of .5 oz CSM looks like after 3 hours of grinding it off. (Kind of reminds me of the 80's!)
I will say that given the amount of effort it took to remove a little bit of LIGHT cloth that was BADLY epoxied to the substrate, I have a whole new level of confidence in the rest of the boat, laid up w/ much heavier cloth, and bonded thorougly w/ epoxy!!

1 comment:

  1. I feel your pain. We glassed in 4 stiffeners and found that they did not bond correctly. Off it goes...Grind, grind, grind. What a mess.

    ReplyDelete